DRAFT FOR REVIEW BY THE DESIGN PROFESSIONAL OF RECORD. Prepared 2026-09-10 by Advanced Formliners from an intake completed by Advanced Formliners guide specification. Not sealed. No licensed professional has reviewed this document. Bracketed text marks a decision left open. SECTION 03 47 13 TILT-UP CONCRETE , NOTES TO THE SPECIFIER (delete before issue) 1. This is a draft for the design professional of record to review, edit, and take responsibility for. It is not sealed and no licensed professional has reviewed it. Text in [square brackets] is a selection still to be made; text in is a value to insert. 2. Structural design criteria, loads, and deflection limits are not written here. The section points at the contract drawings, or at delegated design, as chosen on the intake. 3. Standards are cited by designation. The section requires compliance with PCI manuals and specifications by name and does not reproduce their text; keep them available to the bidders. 4. PCI Architectural Certification category: The work asks for more than one mixture or texture on a unit, or shaped faces beyond flat panels with reveals, which is the Category AB profile. AB producers demonstrate multiple face mixtures, white cement capability, and returns cast in one pour. 5. Tilt-up panels are site cast. The plant certification articles are replaced with contractor qualification and site casting requirements; finish, thin brick, and formliner articles are the same as for plant-cast work. PART 1 GENERAL 1.1 SUMMARY A. Section includes site-cast tilt-up architectural concrete: Tilt-up panels. 1. Clay thin brick units embedded in the concrete face during casting, with formliners that locate the brick and form the joints. 2. Formliner-cast textured finish on exposed concrete faces. 3. Connections, anchors, inserts, and accessories cast into the units. B. Related requirements: 1. Section 01 00 00, General Requirements, applies to this Section. 2. [Section 03 30 00 Cast-in-Place Concrete] [Section 05 12 00 Structural Steel Framing] [Section 07 92 00 Joint Sealants]. 3. Section 04 20 00 Unit Masonry, for field-laid brick adjacent to the embedded thin brick, if any. 1.2 REFERENCES A. The following documents form part of this Section to the extent referenced. The latest edition in force at the date of the Contract applies unless a specific edition is named. B. Precast/Prestressed Concrete Institute (PCI): 1. PCI MNL-117, Manual for Quality Control for Plants and Production of Architectural Precast Concrete Products. 2. PCI MNL-135, Tolerance Manual for Precast and Prestressed Concrete Construction. 3. PCI MNL-120, PCI Design Handbook. 4. PCI MNL-122, Architectural Precast Concrete. 5. PCI MNL-127, Erectors Manual: Standards and Guidelines for the Erection of Precast Concrete Products. 6. PCI Plant Certification Program and PCI Architectural Certification categories. 7. PCI Field Certification (Erector) Program. 8. PCI RP-152, Recommended Practice for Embedded Clay Thin Brick in Precast Concrete, including Appendix A, PCI Specification for Embedded Clay Thin Brick. C. American Concrete Institute (ACI): 1. ACI 301, Specifications for Concrete Construction. 2. ACI 318, Building Code Requirements for Structural Concrete. 3. ACI 211.1, Standard Practice for Selecting Proportions for Normal, Heavyweight, and Mass Concrete. 4. ACI 551.1R, Guide to Tilt-Up Concrete Construction, and ACI 551.2R, Design Guide for Tilt-Up Concrete Panels. D. ASTM International: 1. ASTM A615/A615M, A706/A706M, and A1064/A1064M, reinforcing bars and welded wire reinforcement. 2. ASTM A36/A36M, A276, A307, F3125/F3125M, A123/A123M, A153/A153M, structural and connection steel and its coatings. 3. ASTM C33/C33M, C150/C150M, C595/C595M, C618, C989/C989M, C1240, C1602/C1602M, concrete materials. 4. ASTM C260/C260M, C494/C494M, C1017/C1017M, C979/C979M, admixtures and pigments. 5. ASTM C1107/C1107M, nonshrink grout. ASTM C881/C881M, epoxy adhesives. ASTM C920, elastomeric sealants. 6. ASTM C31/C31M, C39/C39M, C143/C143M, C231/C231M, C138/C138M, C1064/C1064M, field and laboratory testing of concrete. 7. ASTM C1088, Thin Veneer Brick Units Made from Clay or Shale. 8. ASTM C67/C67M, C373, C666/C666M, C650, E488/E488M, test methods referenced for thin brick, as modified in PCI RP-152 Appendix A. E. American Welding Society (AWS): AWS D1.1/D1.1M, D1.4/D1.4M, and D1.6/D1.6M. 1.3 DEFINITIONS A. Architect: the design professional named in the Conditions of the Contract, whose review and acceptance are required where this Section says so. B. Design reference sample: a small sample, produced by the producer from the specified materials, that establishes the intended color, texture, and finish before production begins. C. Mockup: a full-size unit or assembly produced with production methods, used to confirm appearance, tolerances, and construction before production units are cast. D. Thin brick: a fired clay unit not less than 1/2 in. and not more than 1 in. thick, embedded in the concrete face during casting so that the concrete forms the bond, with no adhesive or mortar setting bed. E. Formliner, brick: an elastomeric or plastic liner with pockets that hold each thin brick in position and form the joint between units. Single-use and multi-use liners are both acceptable where they meet the requirements of this Section. F. Formliner, textured: a liner attached to the form face that casts a pattern, relief, or texture into the concrete. G. Exposed face: any surface of a unit visible in the completed work, including returns, reveals, and soffits. 1.4 PREINSTALLATION MEETING A. Convene a meeting at the Project site before production , attended by the Contractor, the concrete subcontractor, the Architect, and the trades whose work connects to the panels. B. Review the approved samples and mockup, the finish acceptance criteria and viewing distance, the sequence of casting and erection, the connection and bracing plan, joint and sealant coordination, protection of finished faces, and the repair procedure and who approves repairs. C. Review thin brick delivery, blending across pallets, the brick and liner tolerance stack-up, joint width and profile, and the pull-out and freeze-thaw test reports. D. Review formliner sheet layout, seam placement relative to reveals and panel joints, pattern orientation, and the number of uses the liner is rated for. 1.5 ACTION SUBMITTALS A. Product data: for each material, admixture, pigment, reinforcement, connection component, insulation, formliner, thin brick, form-release agent, sealer, and repair material. B. Shop drawings: unit elevations, sections, and dimensions; reinforcement and prestressing; connections, inserts, and lifting devices; joint locations and widths; finish designation for each face; reveal and formliner layout; handling and erection sequence; and the relationship of each unit to adjacent construction. Show every exposed face and identify which are finished and which are returns. C. Design reference samples: 1. Sets of three, approximately 12 by 12 by 2 in., for each color, texture, and finish, including one set with the specified thin brick, joint profile, and joint color, before production begins. Samples show the range of color and texture to be expected. 2. Where samples are rejected, resubmit until the Architect accepts one set. The accepted set is the design reference sample and is kept at the plant and on site. D. Thin brick samples: a minimum of five units of each color and blend, from the production run, showing the range of color and texture, with a coursing layout for each bond pattern. E. Formliner samples: a manufacturer sample of the specified pattern, and a cast sample from the design reference sample set showing the pattern at true relief. F. Mixture designs: proportions and material sources for each face and backup mixture, with the trial batch results that support them. 1.6 INFORMATIONAL SUBMITTALS A. Contractor qualification: evidence of at least three completed tilt-up projects of similar size and finish in the last five years, with references. B. Welder qualifications per AWS D1.1/D1.1M and D1.4/D1.4M, current within the period the program requires. C. Material certificates: for cement, aggregates, admixtures, pigments, reinforcement, prestressing strand, connection steel and coatings, insulation, grout, and sealer. D. Test reports: concrete trial batches; aggregate soundness and reactivity; and the plant quality control records for production units when requested. E. Thin brick manufacturer certificate of compliance with ASTM C1088, Grade Exterior, Type TBX, and with the PCI Specification for Embedded Clay Thin Brick (PCI RP-152 Appendix A), with test reports from an independent laboratory for dimensional tolerances, modulus of rupture, absorption, efflorescence, freeze-thaw resistance on assembled specimens, pull-out strength before and after freeze-thaw, and chemical resistance. Where the manufacturer's product varies from the specification, submit the manufacturer's letter of variance for the Architect's review before ordering. F. Formliner manufacturer data: pattern, relief depth, draft, sheet size, material, rated number of uses, and recommended form-release agent. G. Erection and bracing plan, and the lifting and handling procedure for each unit type. H. Repair procedure and materials, submitted before the first repair is made. 1.7 QUALITY ASSURANCE A. Quality control: in accordance with ACI 301, with the additional finish and sampling requirements of this Section. B. Welding: qualified procedures and welders per AWS D1.1/D1.1M for structural steel and AWS D1.4/D1.4M for reinforcing steel. C. Mockup: 1. Cast a full-size mockup unit of each finish, showing the thin brick, bond, corner condition, and joint profile, showing the formliner pattern and a liner seam, using production methods and materials, before production begins. 2. The accepted mockup establishes the range of color, texture, and workmanship. [Retain it until Substantial Completion.] [Incorporate it into the Work where shown.] D. Finish acceptance: 1. Production units are judged against the accepted mockup, viewed in daylight, without magnification, at a distance of 20 feet. 2. Color and texture within the range of the accepted standard, with no unit that reads as a different mixture at the stated distance. Cracks, chips, spalls, honeycomb, form-line offsets, and staining are unacceptable on exposed faces except as the repair procedure allows. 1.8 DELIVERY, STORAGE, AND HANDLING A. Protect finished faces after stripping from staining, construction traffic, and weather until the Work is complete. B. Deliver thin brick on pallets identified by color, blend, and production run. Store dry and covered. Draw units from several pallets at once during setting so that color is blended across every unit. C. Store formliners flat, out of sunlight, and clean; damaged or distorted liners are not used on exposed faces. 1.9 SEQUENCING AND SCHEDULING A. Do not begin production units until the design reference samples and the mockup have been accepted in writing. B. Order thin brick in one release for the full quantity of each color, including corners and special shapes, so that all units come from the same production period. Allow for coursing waste and for the test specimens required by Part 2. PART 2 PRODUCTS 2.1 PERFORMANCE REQUIREMENTS A. Structural performance: as indicated on the Contract Drawings. Design lifting devices and connections for handling, shipping, and erection stresses in addition to the loads indicated. B. Thermal and moisture movement: provide for movement at joints and connections so that restraint does not crack the units or damage adjacent construction. C. Durability: [air entrain concrete in exposed faces for freeze-thaw exposure] [freeze-thaw exposure does not apply at the Project location]. 2.2 REINFORCEMENT AND PRESTRESSING A. Reinforcing bars: ASTM A615/A615M Grade 60, or ASTM A706/A706M where welded. Welded wire reinforcement: ASTM A1064/A1064M. B. Where cover to an exposed face is less than 1-1/2 in., or where the face is acid etched or sandblasted, use [galvanized reinforcement per ASTM A767/A767M] [epoxy-coated reinforcement per ASTM A775/A775M] [stainless steel reinforcement] to prevent rust staining. Non-corroding spacers and chairs only. C. Supports: plastic or stainless steel where they will be within 1 in. of an exposed face; no bare steel touching an exposed face. 2.3 CONNECTION MATERIALS A. Structural shapes, plates, and bars: ASTM A36/A36M. Bolts: ASTM A307 or ASTM F3125/F3125M as indicated. Anchor and headed studs: ASTM A108, welded per AWS D1.1/D1.1M. B. Finish: hot-dip galvanized per ASTM A123/A123M or A153/A153M where exposed to weather or embedded within 1-1/2 in. of an exposed face; zinc-rich touch-up of field welds and damaged coating. Where connections are exposed in the finished work, stainless steel per ASTM A276, Type 304 or 316 as indicated. C. Inserts and lifting devices: as selected by the producer for the loads and the unit geometry, of a type that leaves no ferrous metal within 1 in. of an exposed face after erection. D. Bearing pads: elastomeric, of the durometer and thickness on the shop drawings; nonshrink grout per ASTM C1107/C1107M where bearing is grouted. 2.4 CONCRETE MATERIALS A. Portland cement: ASTM C150/C150M, [white] [gray] cement for face mixtures, of one type and one source for the duration of the Work. Blended cement per ASTM C595/C595M where the producer proposes it, subject to acceptance of the design reference sample made with it. B. Supplementary cementitious materials: fly ash per ASTM C618, slag cement per ASTM C989/C989M, silica fume per ASTM C1240. Use in face mixtures only where the accepted design reference sample was made with the same materials and proportions. C. Aggregates: ASTM C33/C33M, from one source for the duration of the Work. Face aggregates are selected to match the accepted design reference sample and are free of iron pyrites and other staining minerals. D. Water: ASTM C1602/C1602M. E. Admixtures: air entraining per ASTM C260/C260M; water reducing, retarding, and accelerating per ASTM C494/C494M; high-range water reducing per ASTM C1017/C1017M. No admixture containing calcium chloride. F. Pigments: ASTM C979/C979M, inorganic, from one manufacturer for the duration of the Work. 2.5 CLAY THIN BRICK UNITS A. Thin brick: fired clay units per ASTM C1088, Grade Exterior, Type TBX, and complying with the PCI Specification for Embedded Clay Thin Brick (PCI RP-152 Appendix A) for dimensional tolerances, physical properties, and testing on assembled specimens. Where ASTM C1088 and the PCI specification differ, the more stringent requirement governs. B. Basis of design: [insert manufacturer], color or blend [as selected from the manufacturer's full range]. Products of Endicott, MetroBrick, Summitville, General Shale, and King Klinker that meet this Section may be proposed. C. Face size: [Modular, 2-1/4 by 7-5/8 in.] [Norman, 2-1/4 by 11-5/8 in.] [Closure modular, 3-5/8 by 7-5/8 in.] [Utility, 3-5/8 by 11-5/8 in.]. Thickness not less than 1/2 in. and not more than 1 in., and consistent within the tolerance of the PCI specification across the order. D. Special shapes: corners, edge caps, and edge-cap corners of the same body and finish as the field units, at every outside corner and every exposed panel edge where a full brick face is required. E. Back surface: scored, combed, wire-roughened, ribbed, keybacked, or dovetailed, and of the same texture as the units on which the pull-out and freeze-thaw tests were run. A smooth back is not acceptable. F. Properties, tested as thin brick, not as full brick: modulus of rupture not less than 250 psi; 24-hour cold water absorption not more than 6 percent for unglazed units (not more than 5 percent per ASTM C373 for glazed units); rated not effloresced; no deterioration after 300 cycles of ASTM C666 on assembled specimens; pull-out strength from the concrete not less than 150 psi before and after freeze-thaw testing per the modified ASTM E488 method; rated not affected in the modified ASTM C650 chemical resistance test. G. Testing: assembled specimens, sample sizes, and modified methods as described in PCI RP-152 Appendix A, with the number of specimens the appendix requires. Reports not older than [two] years, or for the production run where the Architect requires it. H. Bond pattern: [half (running) bond] [third bond] [stacked bond] [as indicated on the drawings]. I. Joints: [3/8 in.] wide, [raked] [concave] [flush] [vee] [weathered] profile, formed by the liner with the face concrete, not pointed. Joint color: [match design reference sample], produced by the face mixture; no applied mortar or stain. J. Brick formliner: an elastomeric or plastic liner with pockets sized to the brick tolerance range, holding each unit to the face without rotation or float, and forming the joint profile specified. Basis of design: Advanced Formliners, Sparta, Wisconsin, Solocast (single use) or Flex2Fit (multiple use), with pocket dimensions matched to the brick supplied. Liners of another manufacturer that meet this paragraph may be proposed under Division 01. K. Coursing: lay out brick coursing on the shop drawings so that joints align across panel joints, corners turn with full corner units, and cut units are avoided on exposed faces. Where a cut is unavoidable, place it at a reveal or a panel joint, never at a corner. 2.6 TEXTURED FORMLINERS A. Formliner: [insert pattern name and code], basis of design Advanced Formliners, Sparta, Wisconsin, Solocast Seamless line. Liners of another manufacturer producing the same pattern, relief, and draft may be proposed under Division 01 and are accepted only on a cast sample matched to the design reference sample. B. Material: elastomeric (polyurethane) for multiple uses, or a single-use plastic liner, as the producer proposes for the number of casts required. Draft on every relief face not less than the manufacturer publishes for the pattern, and in no case less than 1:8 unless the pattern is specifically designed for stripping at a lesser draft. C. Layout: lay out liner sheets on the shop drawings with seams at reveals, rustications, or panel joints where the pattern allows. Where a seam must fall within a field, butt sheets tightly, match pattern registration, and seal the seam so that no fin or offset shows on the cast face at the acceptance distance. D. Uses: retire a multi-use liner before the pattern softens, fills, or tears; the cast face of the last unit must match the accepted mockup. Do not reuse a single-use liner. E. Form-release agent: compatible with the liner material and the finish, applied thinly and evenly, and not one that stains or interferes with a sealer or coating specified elsewhere. 2.7 CONCRETE MIXTURES A. Proportion mixtures per ACI 211.1 and trial batches. Face mixture and backup mixture may differ; the face mixture is not less than 1 in. thick after consolidation, and thicker where the finish removes surface material. B. Compressive strength: not less than 4,000 psi at 28 days, or as the structural drawings require, whichever is greater. C. Air content of exposed-face concrete: [4 to 6 percent for freeze-thaw exposure], measured per ASTM C231/C231M. D. Water-cementitious materials ratio: not more than 0.45 for exposed-face concrete, and not more than 0.40 where the face is exposed to de-icing salts. E. Consistency: as the producer establishes for full consolidation without segregation; self-consolidating concrete may be used where the design reference sample was made with it. F. Face mixture at thin brick: proportioned to flow into the joint pockets of the liner and fill them completely without voids, and with an aggregate top size that passes freely between units at the joint width specified. G. One source for cement, aggregate, and pigment for the duration of the Work; a change of source requires a new design reference sample and acceptance. 2.8 FORMS AND MOLDS A. Forms: rigid, dimensionally stable, and tight, producing units within the tolerances of Article 2.10, with the corners, reveals, drips, and edges shown on the drawings. Form face material for exposed faces free of defects that would transfer to the concrete. B. Chamfers, reveals, and rustications: as detailed, with draft on every face that is stripped past; no sharp arrises on exposed edges unless detailed and accepted on the mockup. C. Liner attachment: fixed to the form so that the liner does not lift, shift, or wrinkle under placement; liner joints and edges sealed against paste leakage. D. Form-release agent: one that leaves no residue affecting color, bond of finishes or sealers, or the appearance of the exposed face. 2.9 FABRICATION A. Cast panels on a prepared casting slab with a bond breaker that does not stain or affect the finish, in the sequence and with the lifting and bracing inserts on the approved shop drawings. B. Place the face mixture against the form face first where a separate backup mixture is used, and place the backup before the face mixture reaches initial set so that the two bond. C. Set thin brick into the liner pockets by hand, drawing units from several pallets, oriented for the bond pattern, with every corner and edge condition using the special shapes specified. Confirm that no unit is tilted, proud, or missing before concrete is placed. Keep brick faces clean of paste; where paste reaches a face, remove it before it hardens. D. Cure units so that color is uniform across each unit and from unit to unit; do not let part of a unit dry faster than the rest. Steam curing, where used, is uniform across the unit. E. Strip forms and liners at a strength that does not damage arrises, relief, or brick edges. Do not pry against an exposed face. F. Identify each unit with its shop drawing mark on a face that is concealed in the completed work. 2.10 FABRICATION TOLERANCES A. Fabricate panels within the tolerances of ACI 301 and ACI 117 for architectural concrete, unless a tighter tolerance is shown on the drawings. B. Thin brick placement: joint width within plus or minus 1/16 in. of the specified width; units flush to the face plane within 1/16 in.; alignment of joints across a unit face within 1/8 in. in 10 ft, and across a panel joint within 1/8 in. C. Liner seams and pattern registration: no offset at a seam greater than 1/16 in. on the cast face, and pattern alignment across a panel joint within 1/8 in. where the pattern is continuous. D. Surface flatness of smooth exposed faces: within 1/8 in. in 10 ft; form-line offsets within 1/16 in. on exposed faces. 2.11 FINISHES A. Finish each exposed face as scheduled on the drawings and matched to the accepted mockup and design reference sample. Finish returns and soffits to match the adjacent face unless another finish is scheduled. B. Embedded thin brick: after stripping, joints are clean and uniformly profiled; brick faces are free of paste film after the cleaning of Article 2.12; no missing, broken, or replaced units on exposed faces except by the repair procedure. C. Formliner texture: full relief, crisp arrises, no bug holes larger than the mockup shows, no fins or paste bleed at seams, and pattern orientation as shown. D. Repairs: only by the accepted repair procedure and materials, matched in color and texture, and invisible at the acceptance viewing distance. Units with repairs that fail this test are rejected. 2.12 SOURCE QUALITY CONTROL A. Field quality control of casting per ACI 301, with the finish inspections this Section adds. B. Concrete testing: sample and test each mixture per ASTM C31/C31M, C39/C39M, C143/C143M, C231/C231M, and C1064/C1064M at the frequency of ACI 301, and at not less than one set per day of casting for exposed-face concrete. C. Thin brick: verify each delivery against the manufacturer certificate, measure a sample of units for dimensional tolerance per the modified ASTM C67 procedure in PCI RP-152, and reject lots outside tolerance before setting. D. Cleaning after stripping: remove form-release residue, paste film, and curing compound from exposed faces by the method accepted on the mockup; no acid on brick faces or metal, and no method that alters color or texture. E. Architect inspection: the Architect may inspect units at the site at any stage. Acceptance of a unit at the casting bed does not waive rejection of a unit damaged afterwards. PART 3 EXECUTION 3.1 EXAMINATION A. Examine supporting structure, bearing surfaces, anchors, and embedded items for location, elevation, and condition before erection. Report variances that would put units outside the erection tolerances, and do not proceed until they are corrected. B. Verify that field dimensions match the shop drawings, and that adjacent work (field-laid masonry, windows, flashings) is coordinated with the joints and reveals of the units. 3.2 LIFTING AND SETTING A. Erect units per PCI MNL-127 and the accepted erection and bracing plan, by the Contractor, with lifting devices, rigging, and crane positions that do not overstress the units. Set each unit level, plumb, and to line on shims and bearing pads, and brace it until the permanent connections are complete. B. Connections: weld, bolt, or grout per the shop drawings. Protect exposed faces from weld spatter and heat; clean and coat field welds and damaged galvanizing with zinc-rich coating. Grout bearing and connection pockets solid and cure the grout. C. Do not field cut, core, or drill units except where the shop drawings show it or the producer approves it in writing. D. Joints: maintain the joint width shown, [3/4 in. typical] uniform along the full length, with backer rod and sealant by others under Section 07 92 00. 3.3 ERECTION TOLERANCES A. Set panels within the tolerances of ACI 117 for precast and tilt-up elements, and within the joint width shown. B. Jog between adjacent exposed faces at a joint not more than 1/4 in. for smooth faces, and not more than 1/8 in. where thin brick or a formliner pattern continues across the joint. C. Where the structure is out of tolerance, do not force units to line; report and resolve before setting. 3.4 FIELD QUALITY CONTROL A. The Owner may engage a testing agency to inspect erection, connections, welds, and grout. Field welds are visually inspected and, where the drawings require, tested per AWS D1.1/D1.1M. B. Finish inspection after erection: the Architect reviews exposed faces at the acceptance viewing distance in daylight and identifies units for repair or replacement. 3.5 REPAIRS A. Repair damage only by the accepted procedure, using materials matched to the unit and the finish, by workers who repaired the mockup or the first accepted repair. Repairs must be invisible at the acceptance distance; otherwise the unit is replaced at no change in the Contract Sum or Time. B. Missing or broken thin brick: replace with units from the same production run set in a matching bonding material, with joints matched to the adjacent liner-formed joints; a visible patch is not accepted. C. Cracks on exposed faces: reviewed by the Architect. Structural cracks are cause for rejection. Non-structural cracks may be repaired by epoxy injection per ASTM C881/C881M and finished to match only where the Architect accepts the repair. 3.6 CLEANING AND PROTECTION A. Clean exposed faces after erection by the method accepted on the mockup, starting with water and mild detergent and escalating only with the Architect's acceptance. No acid on thin brick faces, connections, or adjacent metal. Protect adjacent materials from run-off. B. Protect finished faces from staining, sealant smears, weld spatter, and construction traffic until Substantial Completion. Remove protection and leave surfaces clean. C. Water repellent: [apply a penetrating silane or siloxane sealer under Section 07 19 00 after cleaning, accepted first on a sample area for appearance] [not required]. END OF SECTION 03 47 13